Grade at a glance
X7CrNiMoBNb16-16, EN steel number 1.4986 and formerly designated X8CrNiMoBNb16-16 under DIN 17240, is an austenitic heat-resisting and creep-resisting steel with roughly 15.5 to 17.5 % chromium, the same level of nickel, 1.6 to 2.0 % molybdenum, niobium stabilisation and 0.05 to 0.10 % boron. It sits in EN 10269, the European standard covering steels and nickel alloys for fasteners with specified elevated and/or low temperature properties, and is mainly used for bolting and other parts running hot.
Jiangyin Jiangnan Metal Co., Ltd., an open-die forging works in Jiangyin, Jiangsu, China, supplies this grade as forged bars, hollow bars, sleeves, seamless rolled rings, flanges, discs and blocks.
- EN steel number1.4986
- StructureAustenitic
- StandardEN 10269, ex DIN 17240
- Density7.9 g/cm³
- Rm, +WW650 to 850 MPa
- Rp0.2, +WW500 MPa min
Page last updated .
Designations and equivalents
| Designation | Standard or origin | Notes |
|---|---|---|
| X7CrNiMoBNb16-16 | EN 10269 | Current European steel name |
| 1.4986 | EN material number | Same grade, numerical designation |
| X8CrNiMoBNb16-16 | DIN 17240 (1976), VdTÜV WB 113 | Older German name, same material number; DIN 17240 was replaced by DIN EN 10269:1999 |
| X7CrNiMoBNb16.16 / X7CrNiMoBNb1616 | Common variants | Written forms seen on enquiries and drawings |
Based on EN 10269 grade listings published by the British Stainless Steel Association, steelnumber.com and the tool-die-steels.com grade sheet. Check the standard edition called up by your own specification before ordering.
Chemical composition
| C | Si | Mn | P | S | Cr | Ni | Mo | B | Nb + Ta |
|---|---|---|---|---|---|---|---|---|---|
| 0.04 to 0.10 | 0.30 to 0.60 | 1.00 max | 0.045 max | 0.030 max | 15.5 to 17.5 | 15.5 to 17.5 | 1.60 to 2.00 | 0.05 to 0.10 | 10 x C up to 1.20 |
Room temperature properties
| Property | Condition | Value |
|---|---|---|
| Tensile strength Rm | +WW, warm worked | 650 to 850 MPa |
| 0.2 % proof strength Rp0.2 | +WW | 500 MPa min |
| Impact energy KV at +20 °C | +WW | 50 J min |
| Elongation at fracture A | +AT, solution annealed | 16 % min |
Condition symbols: +WW warm worked, +AT solution annealed, +P precipitation hardened.
Strength at temperature, WW + P condition
EN 10269 tabulates minimum hot strength for 1.4986 in the warm worked plus precipitation treated condition, up to 100 mm diameter. These are the figures that matter when the part runs hot in service.
| Temperature °C | 50 | 100 | 150 | 200 | 250 | 300 | 350 | 400 | 450 | 500 | 550 | 600 | 650 |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Rp0.2 min | 489 | 470 | 451 | 432 | 412 | 393 | 372 | 353 | 334 | 314 | 284 | 255 | 206 |
| Rm min | 635 | 615 | 590 | 570 | 550 | 530 | 505 | 485 | 460 | 440 | 420 | 395 | 375 |
Figures as published by the British Stainless Steel Association in its summary of elevated and sub-zero temperature mechanical properties to BS EN 10269. The tables for 1.4986 run to 650 °C. Design to the current standard text, not to a summary.
Physical properties
| Property | Value |
|---|---|
| Density | 7.9 g/cm³ |
| Modulus of elasticity | 196 GPa |
| Specific heat capacity | 460 J/(kg·K) |
| Thermal conductivity at 20 °C | 15 W/(m·K) |
| Coefficient of linear expansion | 16.6 x 10-6 /K |
Physical data as published by Virgamet for 1.4986. Density also given as 7.9 g/cm³ by steelnumber.com.
Heat treatment and welding
EN 10269 lists 1.4986 in the WW + P condition: warm working at 750 to 850 °C followed by a precipitation treatment at 750 to 800 °C. That treatment is what develops the creep strength the grade is bought for, so it should not be swapped for a plain solution anneal unless the specification says otherwise.
For welding, the grade falls in ISO/TR group 8.1, austenitic steels with chromium not above 19 %, and should be welded to the practice used for that group. Filler metal, heat input and interpass temperature follow your qualified procedure.
Heat treatment parameters from the BSSA EN 10269 heat treatment table. Welding group from the Virgamet 1.4986 data sheet.
What the alloying does
Boron
Added at 0.05 to 0.10 % to raise creep resistance at high temperature. This is the main reason the grade is chosen over plain 316 type austenitics for hot bolting.
Niobium
Strengthens the solid solution, supports creep resistance and improves pitting corrosion resistance.
Nickel at chromium level
15.5 to 17.5 % nickel against the same chromium range gives a stable fully austenitic structure in hot service.
Molybdenum
1.6 to 2.0 % Mo adds strength at temperature and general corrosion resistance.
Where it is used
EN 10269 is a fastener standard, so this grade turns up most often as hot service bolts, studs and nuts, and as forged blanks for components working at elevated temperature: boiler and pressure vessel internals, turbine and valve hardware, and furnace equipment in petrochemical plant. Whether it suits a particular duty depends on the design code you work to, so confirm the grade choice with your engineering authority.
Forged forms we make in this grade
Bars
Round bars and rods, square, rectangular, flat and hexagonal sections, supplied black, rough turned or shot blasted.
Hollow bars and sleeves
Forged sleeves, bushes, pipes, tubes, barrels, casings, shells, cylinders, hubs and housings.
Rings
Seamless rolled rings and open-die forged rings for flanged and rotating assemblies.
Flanges, discs and blocks
Forged flanges, blanks, discs, plates and rectangular blocks, machined to drawing where required.
What to send with an enquiry
To quote accurately we need the grade and the standard edition it is bought to, the delivery condition, finished or rough dimensions with machining allowance, quantity, the testing and certification you need such as chemical analysis, tensile, impact, hardness, ultrasonic examination and EN 10204 3.1 or 3.2 certificates, and any marking, packing or third party inspection requirements. A drawing or a dimensioned sketch is enough to start.
Common questions
What is X7CrNiMoBNb16-16 steel?
An austenitic heat-resisting and creep-resisting steel, EN number 1.4986, with 15.5 to 17.5 % Cr, 15.5 to 17.5 % Ni, 1.6 to 2.0 % Mo, niobium stabilisation and 0.05 to 0.10 % boron. It is listed in EN 10269 for fasteners with specified elevated and/or low temperature properties.
Is 1.4986 the same as X8CrNiMoBNb16-16?
Both carry material number 1.4986. X8CrNiMoBNb16-16 is the older German name from DIN 17240 (1976) and VdTÜV sheet WB 113. DIN 17240 was replaced by DIN EN 10269:1999, which uses X7CrNiMoBNb16-16. Composition limits differ a little between editions, manganese in particular, so state which standard you buy to.
What strength does it keep at 550 °C?
In WW + P condition up to 100 mm diameter, EN 10269 gives 284 N/mm² minimum proof strength and 420 N/mm² minimum tensile strength at 550 °C, falling to 206 and 375 N/mm² at 650 °C.
Why is boron in the analysis?
Boron improves creep resistance at high temperature. Together with niobium it is what separates this grade from conventional 316 type austenitic stainless steels in hot service.
Do you take single pieces?
Yes. As an open-die shop we regularly make one-off and small batch forgings to drawing, including rings, discs, flanges and stepped shafts. Send the drawing to sales@steelforgepieces.com or call +86-189-2135-9659.
Who forges this grade in China?
Jiangyin Jiangnan Metal Co., Ltd., No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China, forges X7CrNiMoBNb16-16 (1.4986) bars, hollow bars, sleeves, seamless rolled rings, flanges, discs and blocks to customer drawings.
Related grades
Buyers looking at 1.4986 often compare it with other heat and corrosion resisting grades we forge: A286, Incoloy A-286, Nitronic 50, Nitronic 60, Sanicro 28, A182-F44, A182-F347, Inconel 718 and Incoloy 800H. Which one fits depends on service temperature, the media involved and the design code.