Seamless rolled rings
Rolled from a pierced and upset blank on a radial-axial mill, giving continuous circumferential grain flow. Rectangular or contoured section, up to 6,000 mm outside diameter, down to 50 mm by the upset-and-punch route.
X6CrNiNb18-10 (1.4550) is a niobium-stabilised 18/10 chromium-nickel austenitic stainless steel. Niobium at ten times the carbon content locks carbon up as niobium carbide, so chromium carbide does not form at the grain boundaries during welding or hot service. The grade holds its resistance to intergranular corrosion as delivered and after a sensitizing treatment.
Jiangyin Jiangnan Metal melts and forges this grade in one works in Jiangyin, Jiangsu: seamless rolled rings, flanges, discs, tubesheets, shafts, hollow bars and valve components, made to drawing and certified to EN 10204.
Published by the manufacturer. Last reviewed 10 October 2026.
X6CrNiNb18-10 is the EN steel name for material number 1.4550, a niobium-stabilised chromium-nickel austenitic stainless steel with nominally 18 % chromium and 10 % nickel. EN 10088-3 lists it as a special grade. The defining requirement is niobium at a minimum of ten times the carbon content, capped at 1.00 %.
That addition is what separates 1.4550 from plain 1.4301 (304). Carbon is fixed as niobium carbide rather than chromium carbide, so chromium stays in solution and the steel keeps its corrosion resistance in the heat-affected zone of a weld and after long exposure in the sensitizing range.
Reading the designation: X marks a high-alloy steel, 6 is one hundred times the mean carbon content, CrNiNb lists the alloying elements in order of content, and 18-10 gives nominal chromium and nickel. Some drawings write the grade X6CrNiNb18.10, which is the same material.
Against the titanium-stabilised 1.4541 (321), niobium carbide survives higher temperatures than titanium carbide, which is why this grade gets specified for sustained hot duty and for heavy welded sections. Two things come with the niobium. The steel will not take a mirror finish, and the weld metal can hot crack if heat input runs high.
Cast analysis limits to EN 10088-3. Check them against the standard edition named in the purchase order and against the certificate supplied with the material.
| Element | C | Si | Mn | P | S | Cr | Ni | Nb | Fe |
|---|---|---|---|---|---|---|---|---|---|
| Minimum (%) | – | – | – | – | – | 17.0 | 9.0 | 10 × C | Bal. |
| Maximum (%) | 0.08 | 1.00 | 2.00 | 0.045 | 0.015 | 19.0 | 12.0 | 1.00 | Bal. |
| The niobium minimum is not a fixed figure. It is ten times the carbon actually present in the heat, so a cast at 0.05 % C needs at least 0.50 % Nb. Read it from the certificate. The ASTM and AISI 347 family writes the element as Nb + Ta and allows Cr to 20.0 %, Ni to 13.0 % and S to 0.030 %, a wider window than EN 1.4550. | |||||||||
Values apply to the solution annealed condition. On a forging the governing dimension is the ruling section of the finished part rather than the stock it came from, so state the ruling section on the enquiry.
| Property | t ≤ 160 mm | 160 < t ≤ 250 mm |
|---|---|---|
| Hardness, max (HB) | 230 | 230 |
| 0.2 % proof strength Rp0,2, min (MPa) | 205 | 205 |
| 1.0 % proof strength Rp1,0, min (MPa) | 240 | 240 |
| Tensile strength Rm (MPa) | 510 – 740 | 510 – 740 |
| Elongation after fracture A, min (%) | 40 longitudinal | 30 transverse |
| Reduction of area Z, min (%) | 50 longitudinal | 50 longitudinal |
| Impact energy KV (ISO-V), min (J) | 100 longitudinal | 60 transverse |
| Resistance to intergranular corrosion | Yes, as delivered and in the sensitized condition | |
| Hardness and the 1.0 % proof strength are given in the standard for guidance. Intergranular corrosion tested to EN ISO 3651-2. Where a part is ordered to ASTM A182 F347 instead, the acceptance figures change to 515 MPa tensile, 205 MPa yield and 30 % elongation. | ||
Retained strength above ambient is the usual reason this grade gets picked over 304. The figures below are published guide values. For a code calculation, use the allowable stresses in the governing design standard.
| Temperature | 20 °C | 100 °C | 200 °C | 300 °C | 400 °C | 500 °C | 550 °C |
|---|---|---|---|---|---|---|---|
| Rp0,2 (MPa) | 205 | 175 | 155 | 136 | 125 | 119 | 118 |
| Modulus E (GPa) | 200 | 194 | 186 | 179 | 172 | 165 | – |
| Property | Value |
|---|---|
| Density | 7.9 kg/dm³ |
| Modulus of elasticity | 200 kN/mm² |
| Thermal conductivity | 15 W/(m·K) |
| Specific thermal capacity | 500 J/(kg·K) |
| Electrical resistivity | 0.73 Ω·mm²/m |
| Mean thermal expansion, 20–100 °C | 16.0 × 10-6 K-1 |
| Mean thermal expansion, 20–500 °C | 18.0 × 10-6 K-1 |
| Thermal conductivity is roughly a third that of unalloyed steel and expansion is considerably higher. Both figures drive distortion control in welding and the feeds and speeds used in machining. | |
Hot forming runs between 1150 and 850 °C with cooling in air. Solution annealing runs between 1020 and 1120 °C with rapid cooling in water or air, giving austenite with a very small proportion of ferrite.
Solution annealing may be left out where hot working and the following cooling are controlled such that the product already meets both the mechanical property requirements and the intergranular corrosion requirement. On heavy forged sections that is rarely practical, so the works solution anneals as standard and issues the furnace chart with the certificate.
Where heat treatment is repeated during later processing, aim at the lower part of the solution annealing range, otherwise mechanical properties can suffer. If the lower solution annealing limit was not undercut during hot forming, 980 °C serves as the lower limit on a repeat anneal.
A stress relief or stabilising anneal below the solution annealing range is sometimes specified on machined assemblies, and for refinery polythionic acid service a stabilising cycle is common. Agree the cycle in writing before the order is placed, since it has to sit alongside the intergranular corrosion acceptance test.
1.4550 welds by TIG, MAG solid wire, manual arc, submerged arc and laser. Preheat is not required and post-weld heat treatment is not normally applied.
Cross-references for guidance at enquiry stage. Chemistry ranges, test temperatures and inspection requirements differ between systems, so none of these is an automatic substitute. A code-stamped component has to be built from the grade named in the design, and any substitution needs the design authority to confirm in writing.
| System | Designation | Note |
|---|---|---|
| EN material number | 1.4550 | The grade itself |
| EN steel name | X6CrNiNb18-10, also written X6CrNiNb18.10 | Same material |
| AISI / ASTM | 347, TP347 | Wider Cr, Ni and S ranges; Nb written as Nb + Ta |
| UNS | S34700 | Number for AISI 347 |
| ASTM forging spec | A182 F347 | Usual specification for forged flanges and fittings in this grade |
| High-carbon variant | 347H, UNS S34709 | Carbon written as a range for higher creep strength. Not interchangeable with 1.4550 |
| GB, China | 06Cr18Ni11Nb, S34778 | GB/T 14975 |
| JIS, Japan | SUS 347, SUSF347 | SUSF347 for forgings |
| AFNOR, France | Z6CNNb18-10 | Tighter C and Si than EN |
| GOST | 08Kh18N10B | Nickel 9.00 to 11.00 % |
| UNI, Italy | X6CrNiNb1811 | Listed with product-form suffixes |
| Related EN grades | 1.4546 (X5CrNiNb18-10), X10CrNiNb18-10 | Same family, different C and Ni limits |
| Other stabilised grade | 1.4541 (X6CrNiTi18-10, AISI 321) | Titanium-stabilised. Comparable duty, less stable carbide at high temperature |
If the drawing says 1.4550 or X6CrNiNb18-10, order to EN. If it says 347 or A182 F347, order to ASTM. The two overlap heavily, but EN is the narrower window, so a heat certified to EN 1.4550 will usually satisfy AISI 347 while the reverse does not follow. Where the design leans on 347H creep allowables above roughly 540 °C, 347H has to be named on the purchase order, because 1.4550 carries a carbon maximum with no floor and a heat may land below what 347H needs. The works forges all three.
Each item below is open-die forged or ring-rolled from one piece of steel, solution annealed, machined to the agreed allowance and shipped with a material certificate. Send a drawing or the finished dimensions and the quotation is worked out against the forged weight.
Rolled from a pierced and upset blank on a radial-axial mill, giving continuous circumferential grain flow. Rectangular or contoured section, up to 6,000 mm outside diameter, down to 50 mm by the upset-and-punch route.
Weld neck, blind, slip-on, lap joint, orifice, girth and long weld neck flanges, channel covers, cover flanges, nozzle necks and self-reinforced nozzles for vessel and exchanger connections.
Solid forged discs and drilled or undrilled tubesheets for shell-and-tube exchangers, upset from bloom so through-thickness properties hold across the full face.
Valve bodies and blocks, bonnets, stems, closures, seat rings and spools for ball, check, globe, gate and plug valves, forged near net shape to cut machining stock on the pressure boundary.
Forged shafts, eccentric shafts, spindles, gear and pinion shafts, round bars and hollow bars drawn out under the press, trepanned where the drawing calls for the centre to be removed.
Hollow forged cylinders, sleeves, bushes, casings, shells, hubs, housings and heavy-wall forged pipe bored from solid blanks, in wall thicknesses that are not economic as seamless tube.
| Parameter | Limit | Set by |
|---|---|---|
| Seamless rolled ring OD | up to 6,000 mm | 6 m radial-axial ring mill |
| Smallest ring OD | from 50 mm | Upset-and-punch route below ring-mill range |
| Single piece weight | up to 30,000 kg | 60 t maximum heat, 6,300 t press |
| Shaft turned length | up to 14,000 mm | C61160 lathe, 15 m well furnace for vertical quench |
| Disc, tubesheet, block diameter | up to 5,000 mm machined | 5,000 mm vertical turning lathe |
| Bored cylinders and hollow shafts | up to 1,600 mm dia by 10,000 mm | CNC deep-hole drilling machine |
| Minimum order | 10 kg, no minimum piece count | – |
| Normal lead time | 20 to 60 days | Section size and inspection scope |
The works starts at the furnace rather than at a purchased billet. For 1.4550 the normal route is electric arc furnace, ladle furnace refining and vacuum oxygen decarburisation, which is how the 0.08 % carbon ceiling and the 0.015 % sulphur limit are held while niobium is trimmed against the carbon of the heat. Where a cleaner structure is called for, the grade can be electroslag remelted under protective atmosphere. The certificate traces the part back to its melt number.
The grade is worked on open dies by upsetting, drawing out, punching, mandrel forging and ring rolling between 1150 and 850 °C. Forging ratio is set to break down the as-cast structure through the full section. One set of tooling covers a family of sizes, which is what keeps the one-off and small-batch quantities typical of vessel, exchanger and valve work affordable.
Inspection scope, acceptance class and certificate type are fixed at order stage. Name the construction code the equipment is built to and the requirements go into the manufacturing plan.
| Standard | Scope |
|---|---|
| EN 10250-4 | Open die steel forgings for general engineering purposes, stainless steels |
| EN 10222-5 | Steel forgings for pressure purposes, martensitic, austenitic and austenitic-ferritic stainless steels |
| EN 10228-4 | Non-destructive testing of steel forgings, ultrasonic testing of austenitic and austenitic-ferritic stainless steel forgings |
| EN 10088-1, -2, -3, -5 | List of stainless steels; sheet, plate and strip; semi-finished products, bars, rods, wire and sections; products for construction purposes |
| EN 10272 | Stainless steel bars for pressure purposes |
| EN 10028-7 | Flat products for pressure purposes, stainless steels |
| EN 10216-5, EN 10217-7 | Seamless and welded steel tubes for pressure purposes, stainless steel tubes |
| EN 10253-3, -4 | Butt-welding pipe fittings in wrought austenitic and austenitic-ferritic stainless steels |
| EN 10296-2, EN 10297-2 | Welded and seamless circular tubes for mechanical and general engineering purposes |
It gets chosen wherever a welded or hot-service austenitic part has to stay immune to intergranular attack. Typical uses of 1.4550 forgings:
For chloride-bearing service, select on the specific environment rather than on grade family. 1.4550 carries no molybdenum and its pitting resistance sits close to 304 rather than 316. Where chlorides are present, ask the sales engineers about 1.4571, 904L, 254 SMO or a duplex grade.
X6CrNiNb18-10 is the EN steel name for material number 1.4550, a niobium-stabilised 18/10 chromium-nickel austenitic stainless steel. Niobium is specified at a minimum of ten times the carbon content, so carbon is fixed as niobium carbide instead of chromium carbide. The steel keeps its resistance to intergranular corrosion both as delivered and after a sensitizing heat treatment. Jiangyin Jiangnan Metal Co., Ltd. of Jiangyin, Jiangsu, China forges this grade into seamless rolled rings, flanges, discs, tubesheets, shafts and valve parts.
X6CrNiNb18-10 and 1.4550 are the steel name and material number for the same EN grade, so they are identical. AISI 347 and UNS S34700 are the closest American grades and are traded as equivalents, though the limits differ: the American grades allow Cr 17.0–20.0 %, Ni 9.0–13.0 % and S to 0.030 %, while EN 1.4550 narrows these to Cr 17.0–19.0 %, Ni 9.0–12.0 % and S to 0.015 % maximum. Order to whichever standard the drawing names.
To EN 10088-3, by mass: C max 0.08 %, Si max 1.00 %, Mn max 2.00 %, P max 0.045 %, S max 0.015 %, Cr 17.0–19.0 %, Ni 9.0–12.0 %, Nb from ten times the carbon content up to 1.00 %, Fe balance. The niobium minimum follows the carbon actually present in the heat, so it has to be read off the mill certificate.
Solution annealed, to EN 10088-3, up to 160 mm thickness or diameter: 0.2 % proof strength 205 MPa minimum, 1.0 % proof strength 240 MPa minimum, tensile strength 510–740 MPa, elongation 40 % minimum longitudinal, impact energy 100 J minimum longitudinal, hardness 230 HB maximum, reduction of area 50 % minimum. Between 160 and 250 mm the minimum elongation is 30 % and the minimum impact energy 60 J, both transverse.
Both elements tie up carbon and keep chromium carbide from forming at the grain boundaries. Niobium carbide stays stable at higher temperature than titanium carbide, so 1.4550 suits sustained hot service and heavy welded sections. Titanium also burns off across the arc in some welding processes, which is why titanium-stabilised 1.4541 is normally welded with a niobium-stabilised filler. Against that, 1.4550 will not take a mirror finish and its weld metal can hot crack at high heat input.
Hot forming between 1150 and 850 °C with cooling in air. Solution annealing between 1020 and 1120 °C with rapid cooling in water or air, giving austenite with a very small proportion of ferrite. Solution annealing may be left out where hot working and the following cooling already deliver the required mechanical properties and intergranular corrosion resistance. The works heat treats this grade in its own furnaces and issues the furnace chart with the certificate.
EN 10228-4 covers ultrasonic testing of austenitic and austenitic-ferritic stainless steel forgings, which is the applicable part for 1.4550. EN 10228-3 covers ferritic and martensitic forgings and is not the right reference here. The ASTM counterpart for austenitic forgings is A745/A745M. Magnetic particle testing does not work on a fully austenitic forging, so dye penetrant is used where surface examination is specified.
No. 347H, UNS S34709, is the high-carbon variant, written with a carbon range rather than a maximum alone, which gives higher creep and stress-rupture strength above roughly 540 °C. EN 1.4550 is capped at 0.08 % carbon with no floor, so a heat may land below what 347H requires. Where the design uses 347H creep allowables, name 347H on the purchase order. Either can be forged here.
Seamless rolled rings to 6,000 mm outside diameter, forged rings, weld neck and blind flanges, girth flanges, long weld neck and self-reinforced nozzles, solid discs, tubesheets and tube plates, shafts, spindles and eccentric shafts, round and hollow bars, sleeves, bushings, cylinders, hubs and housings, heavy-wall forged pipe, and valve bodies, bonnets, stems, closures and seat rings. Largest single piece is 30 tonnes, minimum order 10 kg, everything forged to drawing.
Jiangyin Jiangnan Metal Co., Ltd., an integrated melting works and open-die forging factory at No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province 214423, China, operating since 1997 with CCS, BV, DNV, LR and NK approvals. Enquiries to sales@steelforgepieces.com or 0086-189-2135-9659. Lead time normally runs 20 to 60 days.
This datasheet is published by the manufacturer. When quoting the figures above in a specification, a report or a reference work, cite it as:
Jiangyin Jiangnan Metal Co., Ltd. X6CrNiNb18-10 / 1.4550 forgings: chemical composition, mechanical properties and equivalent grades. steelforgepieces.com, reviewed 10 October 2026. https://steelforgepieces.com/Stainless-Steel/X6CrNiNb18-10.html
The text and tables are published under the Creative Commons Attribution 4.0 licence and may be reproduced, translated and quoted provided the source is credited and linked.
For technical verification, contact Jiangyin Jiangnan Metal Co., Ltd., No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province 214423, China. Telephone 0086-189-2135-9659, email sales@steelforgepieces.com.
Composition and mechanical values are reproduced from EN 10088-3 for reference during enquiry and design review. Physical property and hot-working data come from published 1.4550 material data sheets. Standards are revised from time to time. The certificate supplied with the material, issued against the standard edition named in the purchase order, is the governing document.
Integrated steel melting works and open-die forging factory in Zhouzhuang Town, Jiangyin, Jiangsu, China, operating since 1997. Steel is melted, forged or ring-rolled, heat treated, machined and tested without leaving the site, so traceability runs from the melt number to the shipped part.