Grade sheet EN 1.4541 / X6CrNiTi18-10 / AISI 321 Melting, forging, heat treatment and machining in one works, Jiangyin, China +86 189 2135 9659   sales@steelforgepieces.com
Jiangyin Jiangnan Metal Open-die forgings · Seamless rolled rings · Since 1997 Get a quote

Austenitic stainless steel · Titanium stabilised

X6CrNiTi18-10 forgings EN 1.4541 · AISI 321 · UNS S32100 · rings, flanges, shafts, discs and bars forged to drawing

X6CrNiTi18-10 is the EN name for titanium-stabilised 18/10 austenitic stainless steel, material number 1.4541, equivalent to AISI 321 and UNS S32100. The titanium addition, specified at five times the carbon content up to 0.70 per cent, binds carbon as titanium carbide so the steel stays resistant to intergranular corrosion before and after welding. Solution annealed, it gives 500 to 700 N/mm2 tensile strength, 190 N/mm2 minimum proof strength and 40 per cent minimum elongation, with a PREN of 17.0 to 19.0 and a service limit near 550 °C.

Jiangyin Jiangnan Metal melts this grade in its own furnaces and forges it on site. Heats run to 60 tonnes, presses to 6,300 tonnes, rings to 6,000 mm outside diameter and single pieces to 30 tonnes. Minimum order is 10 kg.

Grade summaryEN 10088-3
EN number
1.4541
EN name
X6CrNiTi18-10
AISI / UNS
321 / S32100
Structure
Austenitic, titanium stabilised, non-magnetic when annealed
Rm
500 to 700 N/mm2
Rp0.2
190 N/mm2 minimum
Elongation
40 per cent minimum
Hardness
215 HB maximum
Forging
1180 down to 950 °C
Annealing
1020 to 1100 °C, water or air
Certification
EN 10204 3.1 standard, 3.2 witnessed on request
Supply
From 10 kg, 20 to 60 days
01

What 1.4541 is, and why it exists

1.4541 sits in the classic 18/10 austenitic family and differs from plain 1.4301 only by its titanium addition. Hold an unstabilised 18/10 steel in the sensitisation range and chromium carbides form at the grain boundaries, leaving the metal beside them short of the chromium it needs to stay passive. That happens whether anyone intends it or not, because the heat-affected zone of every weld passes through that range. Titanium forms carbides more readily than chromium does, so in 1.4541 the carbon is captured as titanium carbide and the chromium stays in solution. Resistance to intergranular attack is therefore guaranteed in the welded condition as well as the annealed one.

Beyond that, the grade behaves as a general-purpose austenitic. It is non-magnetic when annealed, with relative permeability below 1.3. It keeps good toughness down to cryogenic temperatures, which is why it turns up in liquefied gas work. It resists nitric acid and nitrates well, which is why the nitrogen fertiliser industry has used it for decades. It is very well suited to cold forming by bending, flanging, deep drawing and spinning, and it is suitable for cold heading to EN 10263-5.

A note on DIN 17440. Older drawings often call this grade up under DIN 17440. That standard has been replaced by the EN 10088 series, and every figure on this page follows EN 10088-3. Send the drawing with your enquiry and the equivalence is confirmed in writing before the heat is melted.

For forgings the governing delivery standards are EN 10222-5 for pressure purposes and EN 10088-3 for semi-finished products and bars. Customers working to ASTM specify the same material as ASTM A182 F321. The grade also appears in EN 10028-7 for pressure plate, EN 10216-5 and EN 10217-7 for tubes, EN 10253-3 and EN 10253-4 for butt-welding fittings, and AMS 5645 for bar.

02

Equivalent grades

Cross reference for X6CrNiTi18-10 / 1.4541
StandardDesignation
EN 100881.4541, X6CrNiTi18-10
ASTM / AISIAISI 321, UNS S32100, ASTM A182 F321 for forgings
AMSAMS 5645 bar, AMS 5510 sheet and plate
BS321S31, 321S51
AFNORZ6CNT18-10
JISSUS 321
GB06Cr18Ni11Ti, former designation 0Cr18Ni10Ti
GOST08Kh18N10T, 12Kh18N10T, 06Kh18N10T
PN0H18N10T, 1H18N9T
Other EN and DIN1.4544, X7CrNiTi18-10, X10CrNiTi18-10
Heat-resistant version1.4878, X8CrNiTi18-10, AISI 321H, UNS S32109

The EN and ASTM versions are close but not identical. EN 1.4541 allows silicon up to 1.00 per cent against 0.75 per cent for AISI 321, and AISI 321 adds a nitrogen ceiling of 0.10 per cent that EN 10088-3 leaves unspecified. Where a part has to satisfy both, the heat is aimed at the narrower of the two limits.

03

Chemical composition

Composition in mass per cent, heat analysis
ElementEN 1.4541AISI 321 / UNS S32100
Carbon0.08 max0.08 max
Silicon1.00 max0.75 max
Manganese2.00 max2.00 max
Phosphorus0.045 max0.045 max
Sulphur0.030 max0.030 max
Chromium17.0 to 19.017.0 to 19.0
Nickel9.0 to 12.09.0 to 12.0
Titanium5 x C to 0.700.70 max
Nitrogennot specified0.10 max
Ironbalancebalance

Melting route

This grade is melted in the works rather than bought in as billet. The normal route is the 25 t electric arc furnace, refining in a 25 t or 50 t ladle furnace, then vacuum oxygen decarburisation in the 30 t or 60 t unit where carbon or nitrogen has to be held tight. Electroslag remelting in the 3 t or 6 t protective-atmosphere furnace is available where cleanliness or segregation control governs the acceptance. Maximum heat size is 60 tonnes. Chemistry is checked on an optical emission spectrometer at the furnace, so the certificate starts at the melt number instead of at a supplier's billet.

04

Mechanical and physical properties

Room temperature, solution annealed condition
PropertyValue
Tensile strength Rm500 to 700 N/mm2
Proof strength Rp0.2190 N/mm2 minimum
Elongation A40 per cent minimum
Hardness215 HB maximum
Modulus of elasticity200 GPa
Density7.9 kg/dm3
Thermal conductivity at 20 °C15 W/m·K
Specific heat capacity at 20 °C500 J/kg·K
Electrical resistivity at 20 °C0.73 ohm·mm2/m
MagnetisabilityNon-magnetic when annealed, relative permeability below 1.3
Maximum service temperatureabout 550 °C
PREN17.0 to 19.0

Why other data sheets show different numbers. Property limits depend on the section size and on which standard governs. The values above are the EN 10088-3 figures for bars and semi-finished products. ASTM A182 F321 and EN 10222-5 state their own acceptance values, and heavy sections are agreed case by case. The guaranteed values for your actual ruling section are confirmed at the quotation stage, before the order is placed.

Mechanical testing is carried out in the on-site laboratory on 600 kN and 300 kN universal testing machines to ASTM A370 or ISO 6892, with Charpy V-notch impact testing to minus 60 °C where the specification calls for it.

05

Forging and heat treatment

1.4541 forges well, but it is less forgiving than carbon steel. Thermal conductivity is roughly a third that of unalloyed steel, so the billet has to be brought up slowly and soaked evenly; an uneven soak puts stress into the piece and cracks it. The second rule is to finish the deformation before the temperature drops into the range where sigma phase can form, because that phase takes the corrosion resistance away.

Thermal cycle for open-die forging
StepTemperatureNotes
Heating and soakabout 1150 to 1180 °CSlow, even heating. Billets must be clean, since surface residues attack the steel while it heats
Forging1180 down to about 950 °CFinish above the range where sigma phase forms
Cooling after forgingair or waterCooled quickly
Solution annealing1020 to 1100 °CWater or air quench. A fast quench through the sensitisation range is the point of the operation

Solution annealing is done in the plant's own furnaces. Fourteen are available, from car-bottom furnaces with working chambers up to 8,000 x 2,000 x 2,000 mm down to high-temperature units, plus two well-type furnaces 15 m deep that let long shafts be quenched vertically without bending. Furnace charts are issued with the certificate.

06

Corrosion resistance, and where the grade stops

With a PREN of 17.0 to 19.0, 1.4541 performs well in natural, low-chloride conditions, where a passive film forms in contact with oxygenated water. It handles water vapour to around 400 °C and dilute acids at room temperature, and it is particularly at home in nitric acid and nitrate service. Its defining property is immunity to intergranular attack in the welded condition.

The limits are just as clear and are worth stating plainly rather than glossing over. 1.4541 is not resistant to seawater. Prolonged contact with sodium chloride brings a risk of pitting, and the grade should not be specified for seawater, brine or subsea duty. Continuous service is limited to about 550 °C. Where higher temperatures are needed, 1.4878 or AISI 321H, classified to EN 10095, runs to about 850 °C in a neutral atmosphere.

If the service is seawater, brine or sour, change grade. Suitable alternatives forged in the same works are A182 F44 and 904L for high-chloride process duty, Sanicro 28 for acid service, and A182 F51, A182 F53 or A182 F55 for duplex and super-duplex requirements including NACE MR0175 / ISO 15156.

07

Welding, machining and cold forming

Welding

Weldability is good by all common fusion processes except gas welding. Preheating is not required. Interpass temperature should be kept low, in the region of 150 °C, which limits hot cracking and keeps heat tint down. Recommended fillers are 1.4316 and the niobium-stabilised 1.4551. Post-weld heat treatment is normally unnecessary, since stabilisation is what the titanium is there for, but heat tint and scale must be removed so the passive layer can re-form.

Machining

Machinability is poor. The steel work-hardens quickly and conducts heat badly, so the surface hardens ahead of the tool and the heat stays in the cut. Carbide or high-speed steel tooling, rigid set-ups, positive rake, plenty of coolant and no dwelling are the usual answers. This is allowed for when machining allowances are agreed on forged blanks.

Cold forming

The grade is very well suited to bending, flanging, deep drawing and spinning, and is covered for cold heading and cold extrusion by EN 10263-5.

08

Forged products in 1.4541

Everything is made to the customer's drawing or written specification. There is no stock catalogue; each item comes from a heat melted for the order.

Product forms and the limits that set their size
ProductSize limitSet by
Seamless rolled ringsOD 50 to 6,000 mm6 m, 3 m and 1 m radial-axial ring mills, upset and punch below the mill range
Forged rings and sleevesto 30 t single piece6,300 t, 4,000 t and 2,000 t presses
Forged flangesto drawing, ASME B16.5 and B16.47 profilesPress and ring mill
Forged shafts and spindlesto 14,000 mm turned lengthC61160 horizontal lathe, 15 m well furnace for vertical quenching
Discs, tube sheets and coversto 5,000 mm machined diameter5,000 mm vertical turning lathe
Bored cylinders and hollow barsto 1,600 mm dia x 10,000 mmCNC deep-hole drilling machine
Round bars and blocksto drawingPresses and hammers
Valve bodies, seat rings, stems, blocksto drawingPress plus CNC machining

Parts can be supplied as forged with machining allowance, proof-machined for ultrasonic testing, or finish-machined to drawing. Minimum order is 10 kg, with no minimum piece count, and normal lead time is 20 to 60 days.

09

Where 1.4541 forgings are used

Application fields
IndustryTypical forged parts
Chemical and nitrogen fertiliserVessel rings, flanges, covers, pump and valve parts, pipeline fittings
Food and beverageProcessing and storage equipment components, shafts, sleeves
Cryogenic equipmentFlanges and rings for liquefied gas service, where low-temperature toughness governs
Exhaust and emission controlSilencer and exhaust gas decontamination components
Transport and vehicle constructionStructural and system components
Heat exchangeTube sheets, covers, separator internals
RefiningStabilised-grade components for polythionic acid service
Pulp and paperDigester, liquor tank and machine components
Valves and flow controlBodies, bonnets, seat rings, stems, blocks
10

Testing and certification

Inspection scope for 1.4541 forgings
ItemStandard or detail
Chemical analysisOptical emission spectrometry to ASTM E415, infrared carbon and sulphur to ASTM E1019, handheld PMI
Mechanical testingTensile to ASTM A370 and ISO 6892, Charpy V-notch to minus 60 °C, hardness to ASTM A956 converted per ASTM E140
Ultrasonic testingEN 10228-3, SEP 1921 or ASTM A388, acceptance class as specified
Magnetic particle and visualASTM E709, bore inspection by endoscope
Grain sizeASTM E112 metallography
Intergranular corrosionASTM A262 through an accredited third-party laboratory, reported with the mill certificate
CertificationEN 10204 3.1 as standard, EN 10204 3.2 witnessed by BV, DNV, LR, SGS, TUV or the customer's inspector
Class approvalsCCS, BV, DNV, LR, NK
TraceabilityMelt number through forging, heat treatment and machining to shipment
11

Questions we are asked about this grade

What is X6CrNiTi18-10?

The EN name for titanium-stabilised austenitic stainless steel, material number 1.4541, equivalent to AISI 321 and UNS S32100. Titanium at five times the carbon content, up to 0.70 per cent, ties up carbon as titanium carbide, which keeps the grade resistant to intergranular corrosion before and after welding.

Is X6CrNiTi18-10 the same as AISI 321?

They are equivalent. Two limits differ: EN 1.4541 allows silicon to 1.00 per cent against 0.75 for AISI 321, and AISI 321 sets nitrogen at 0.10 per cent maximum where EN 10088-3 does not specify it. Where both standards apply, the heat is aimed at the tighter limit.

What is the difference between 1.4541 and 1.4878?

1.4878, also called X8CrNiTi18-10 or AISI 321H, is the heat-resistant version with higher carbon and titanium. Classified to EN 10095, it runs to about 850 °C in a neutral atmosphere and has published creep data. Standard 1.4541 is used to about 550 °C.

What is the difference between 321 and 347?

Both are stabilised 18/10 austenitics. 321 uses titanium, 347 uses niobium. Niobium is often preferred for welded assemblies because titanium tends to be lost across the arc. See A182 F347 and AISI 347H.

At what temperature is 1.4541 forged?

Heat slowly and evenly to about 1150 to 1180 °C, forge from 1180 down to about 950 °C, then cool in air or water. Solution anneal afterwards at 1020 to 1100 °C with a water or air quench.

Can 1.4541 be used in seawater?

No. Its PREN of 17.0 to 19.0 is too low and it is not resistant to seawater. Use A182 F44, 904L, Sanicro 28, or duplex and super-duplex grades such as A182 F51, F53 and F55 instead.

Is 1.4541 magnetic?

Not in the solution annealed condition, where relative permeability is below 1.3. Heavy cold work can raise it slightly through deformation martensite.

Which filler metal should be used?

1.4316 or 1.4551. No preheat, interpass temperature held near 150 °C, and normally no post-weld heat treatment. Heat tint must be removed afterwards.

What is the largest 1.4541 forging you can make?

Rings roll to 6,000 mm outside diameter on the 6 m radial-axial mill. The heaviest single piece is 30 tonnes, forged on 6,300 t, 4,000 t and 2,000 t presses from heats of up to 60 tonnes. Shafts turn to 14 m, discs to 5,000 mm diameter.

How is 1.4541 priced, and what is the minimum order?

Every piece is made to drawing, so there is no list price. Minimum order is 10 kg with no minimum piece count, and lead time runs 20 to 60 days from order confirmation. Standard stainless grades such as 1.4541 sit at the lower end of that range because no remelting step is needed. Third-party witnessed inspection and outside corrosion testing need scheduling, so mention them at enquiry stage.

Do you supply finish-machined parts?

Yes. As forged with allowance, proof-machined for ultrasonic testing, or finish-machined to drawing. Heat treatment, machining and testing are all done on site.

Request a price for 1.4541 forgings

Six items give a firm price without a round trip: grade or specification, dimensions or a drawing, quantity, delivery condition, heat treatment and testing requirements, certification type and destination port. Prices normally come back within two working days.

Jiangyin Jiangnan Metal Co., Ltd.
No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China
Telephone, WhatsApp and WeChat: +86 189 2135 9659
Email: sales@steelforgepieces.com
Monday to Saturday, 08:00 to 17:30 China Standard Time

Email a drawing Call the works

Published by Jiangyin Jiangnan Metal Co., Ltd., No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China. First published 12 April 2019. Last reviewed . Compiled from EN 10088-3, EN 10222-5 and published mill data for 1.4541. Values are indicative and do not replace the governing specification or the purchase agreement. Plain-text version of this page: X6CrNiTi18-10.md